Novel Reusable Sponge Could Revolutionize Ocean Oil Spill Cleanup

This is done by performing a two-step surface chemical treatment. In the first step, the foam is impregnated with an ultra-thin, inorganic coating using SIS. To perform SIS, the polymer is alternately exposed to two molecular precursor vapors that cause inorganic materials to grow within the polymer.